The lateral displacement polarization beam splitter prism is composed of a right angle prism and a square prism glued together, and the glued surface is coated with a polarization beam splitter film. It can generate two parallel polarized beams of light, and the lateral displacement of the two beams is determined by the length of the square prism.
Divide the incident light into two parallel linearly polarized beams
UV adhesive bonding
Wave plates can be added to adjust the polarization state of the emitted light
specifications
Dimensional tolerance: ± 0.2mm
Surface quality: 60/40
Passing aperture: >90%
Surface shape: < λ/ 4 @ 632.8nm
Beam deviation: <3 minutes
Chamfer protection: <0.5mmx45 °
Extinction ratio: >100:1
Through parameters: Tp>90%, Ts<1%
Reflection parameter: Rs>99%, Rp<5%
Coated adhesive surface is coated with polarized spectroscopic film, and all outgoing and incoming surfaces are coated with antireflective film
Damage threshold: >500mJ/cm2, 20ns, 20Hz @ 1064nm
The lateral displacement polarization beam splitter prism is composed of a right angle prism and a square prism glued together, and the glued surface is coated with a polarization beam splitter film. It can generate two parallel polarized beams of light, and the lateral displacement of the two beams is determined by the length of the square prism.
Divide the incident light into two parallel linearly polarized beams
UV adhesive bonding
Wave plates can be added to adjust the polarization state of the emitted light
specifications
Dimensional tolerance: ± 0.2mm
Surface quality: 60/40
Passing aperture: >90%
Surface shape: < λ/ 4 @ 632.8nm
Beam deviation: <3 minutes
Chamfer protection: <0.5mmx45 °
Extinction ratio: >100:1
Through parameters: Tp>90%, Ts<1%
Reflection parameter: Rs>99%, Rp<5%
Coated adhesive surface is coated with polarized spectroscopic film, and all outgoing and incoming surfaces are coated with antireflective film
Damage threshold: >500mJ/cm2, 20ns, 20Hz @ 1064nm